after my process of deposition of metals on silicon wafer, i want to go for bulk micromachining process ( TMAH), but hot allign the back side of wafer so that the etching area is exactly under the top side pattren. I do not have the facility of double sided mask alligner. M. Aslam m_aslammalik@hotmail.com