Hi,

 can you please suggest me some vendors for Black Wax as a mask for KOH etch.
Can you please tell me the vendors that are based in US only, since it will be
difficult for me to procure my order if they are outside the US.

  Also can you please suggest me something by which I can remove black wax after
I have etched.

Thanks in advance,

Abhijat Goyal