Plating on stainles steel
Plating on stainles steel
BERAUER,FRANK (HP-Singapore,ex7)
2002-03-21
Ni does not adhere well to stainless steel. It peels off easily,
a fact we use to prepare standalone Ni sheets - the underlying
SS layer can be reused for many re-platings and peelings.

Greetings,
        Frank Berauer
        Senior R&D Engineer
        Hewlett-Packard Singapore


-----Original Message-----
From: Liz Shelley [mailto:lshelley@micrometrics.com]
Sent: Friday, March 22, 2002 3:37 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] Plating on stainles steel


Hello
Does anyone know how I would go about plating a nickel  corrosion coat on
stainless (to be used as a probe)?
I've heard that I must plate with copper first and then nickel.
Any information or source of information will be greatly appreciated.
Liz
_______________________________________________
mems-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply