Dear Ali Razavi (and MEMSNET)

We have some experience of etching lenses in quartz.  Here is a link to a
poster that was presented at a meeting on micro-optics at an IOP meeting
last year (http://www.oxford-instruments.com/pdf/IOPlens.pdf).  See also the
website link below.

http://www.oxfordplasma.de/process/sio_lens.htm

Please contact me if you need more information.

Regards,

Martin Walker BSc(Tech) MSc
Tactical Marketing Engineer
Oxford Instruments Plasma Technology
North End, Yatton,
Bristol BS49 4AP  UK
T. +44 (0) 1934 837031
F. +44 (0) 1934 837001
E. 
W. 

 ###  OXFORD INSTRUMENTS   http://www.oxford-instruments.com/  ###

Unless stated above to be non-confidential, this E-mail and any
attachments are private and confidential and are for the addressee
only and may not be used, copied or disclosed save to the addressee.
If you have received this E-mail in error please notify us upon receipt
and delete it from your records. Internet communications are not secure
and Oxford Instruments is not responsible for their abuse by third
parties nor for any alteration or corruption in transmission.

reply