durusmail: mems-talk: Ultrathin Si wafers
Ultrathin Si wafers
Ultrathin Si wafers
kirt_williams@agilent.com
2002-05-07
> Good day all,
>   Does anyone know where I can purchase a small quantity
> (about 3) of 5"
> ultrathin Si wafers ~100microns thick?
>

It looks like Virginia Semiconductor has some 82-um wafers in stock right now.
See
http://www.virginiasemi.com/products.cfm?cat=54

reply