Hello Tinghui,

you will find more often electroless deposition of Ni on Al instead of
electroplating. If you are looking for literature on electroless Ni
please refer to the website
http://www.pb.izm.fhg.de/avt/050_download/index.html


Best regards

Hermann Oppermann

--

Dr. Hermann Oppermann
Fraunhofer IZM
Gustav-Meyer-Allee 25
D-13355 Berlin, Germany
--------------------------------------------------
phone: +49-30-46403-163, -160
Fax:   +49-30-46403-161
email: hermann.oppermann@izm.fhg.de
--------------------------------------------------
Dept. Chip Interconnection Technologies
Group Optoelectronics, HF and Sensor Integration
http://www.izm.fhg.de/avt/opperm.htm
--------------------------------------------------


gang hong wrote:

>Hi folks,
>
>I want to electroplate Ni on Al(as a seed layer). I
>didn't find relative literature on websites. I wonder
>if it's doable. Any response will be highly
>appreciated. Thanks a lot.
>
>Tinghui
>L/?*Dc5DUFPD HCNR?4?4Dc
>http://sweepstakes.yahoo.com/2002cnuser
>_______________________________________________
>MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

reply