Have you tried the published Tantalum etches, or do you have to avoid use of HF?


 Peter & Judy Wright
wrote:Does anyone know of a wet etch for tantalum nitride? We are using it for
an
underbump metalization at a subcontractor who does not have a dry etch
capability.

Peter Wright