What you are seeing is probably no different from what companies observe with KOH/silica slurries for silicon (wafer) polishing, or for dielectric CMP- chemical mechanical polishing. Perhaps you might contact Rodel Corporation (Delaware, USA) or Westech/IPEC (Phoenix, Arizona, USA). ---R.W. Griffith