Another low-cost quick and dirty method is sandblasting.
It can achieve down to 150um holes, but the edges are ragged
and not very accurate. It works well as ink-feed holes for our
Inkjets, but is not much used eleswhere.

Greetings,
        Frank Berauer
        Senior R&D Engineer
        Hewlett-Packard Singapore


-----Original Message-----
From: Michael D Martin [mailto:michael.martin@louisville.edu]
Sent: Thursday, November 28, 2002 1:10 AM
To: mems-talk@memsnet.org
Subject: Re: [mems-talk] Through holes (vias) in quartz glass 4 " wafer?


You have three options:
1) DRIE (Deep Reactive Ion Etching): This option will require a nice
thick resist. You can contact STS in the UK.
2) Laser Cutting: You can contact Lambda Physik in Germany.
3) Micromilling: We can micromill vias down to ~100 micron diameter.
But we're in Kentucky.

-Good luck
      Mike

>>> Anna-Sara.Hedman@acreo.se 11/27/02 06:41AM >>>
Dear Sir/Madam,

Do you know how to make via holes - i.e. holes through
a quartz glass (fused silica) 4 " wafer, 525 microns thick?

Or do you know anybody else who can do this (in Europe if possible?)
by laser or ultrasonic drilling? Or any other technique?

I need to have approx. 160 holes in each wafer.
The wafer is covered with photoresist (or other masking material)
to mark the location of the through holes,  but also to protect
the bonding surface on the other side from mechanical scratch ...
The hole location is quite important...

I'll  be happy to hear from you soon !

Thanks!

Best regards








_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply