Dear Lucia,
our company Laser Light Technologies has a lot of experience machining Kapton
including drilling holes with accuracy of +/- 3 um. You can find more info about
our capabilities at out web site www.laserusa.com and you also can contact me
via phone or e-mail below.
Regards,
Alex Pozdin,
Director of Engineering