Hi, I think the H2 acts as a reducing agent. With the N2 used as a dilution. Used, in the past, for 'ashing' Chromium: substitute to using O2, which would have volatised the Cr. phil > from: Joseph Chao> date: Tue, 24 Dec 2002 01:30:07 > to: mems-talk@memsnet.org > subject: Re: [mems-talk] forming gas in O2/CF4 etching > > Frank > Could you kindlyl explain to us on the role of forming gas (N2/H2 10%) in > CF4 / O2 PR plasma ashing process. Approximate 15um spacer (PR) removal > under superstructure process in ICP plasma chamber at ~800W RF > > Kind regards > Joseph Chao > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/