You may want to try HTE Labs   http://www.htelabs.com/

Regards,

Tom

-----Original Message-----
From: Alex Pozdin [mailto:apozdin@laserusa.com]
Sent: Friday, January 31, 2003 8:18 AM
To: MEMC chat
Subject: [mems-talk] thick polyimide film on glass


Hello, MEMS Community!
I am looking for the vendor who can coat our borosilicate glass substrates
10X10" with polyimide material 75um thick polyimide material. Desired
thickness variation is less than 10um. Smaller size substrates can be
considered for initial testing.
Regards,
Alex Pozdin,
Director of Engineering
5 Danuser Dr.
Hermann, MO 65041 USA
ph. 573-486-5500
e-mail: apozdin@laserusa.com
fax 573-486-5540


_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply