Hello everyone, I was wondering if anyone knew of a good dielectric material that can withstand an AC voltage of greater that 700 volts? At the same time I am looking at a coating thickness of 1.5 to 2 microns. We have been trying to actuate salt solution (highly conductive KCL) using SU-8 2 and Teflon for microfluidic research purposes but so far most of my efforts have been in vain. I tried SU-8 10 which gave me an approximate thickness of 30 microns and I guess it was too thick. If anyone has had any success with some coating for salt solution, I would appreciate it if you could share that with me. Thanks a bunch in advance, ******************************************************************************* Rajib Ahmed 347 Hopeman Engineering Building Department of Electrical and Computer Engineering University of Rochester Rochester, NY 14627-0167 Email:rajib@ece.rochester.edu Phone#:(585)275-8093 Fax#:(585)273-4919 *******************************************************************************