     Parylene can not be spin coated, but Polymide and B.C.B. can.  In both of
these chemicals you can get photosensitive coatings and after the correct bake
the material is equivalent to parylene in dielectric and thermal qualities.
Suggest you contact Dupont and Arch chemical for info on Polymide.  Try
symposiumonpolymers.com for technical papers on Polymide.  Also contact Dow for
papers on B.C.B.  Bill Moffat

-----Original Message-----
From: Narayanan Unni [mailto:unni@sciences.univ-angers.fr]
Sent: Monday, March 03, 2003 10:49 AM
To: General MEMS discussion
Subject: [mems-talk] Parylene dimer coating


Can anybody tell me if parylene dimer can be spin coated and =
polymerised?
Ideas about dip coating are also welcome
Unni
_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply