Stefan - I wonder if you ever received any useful information in response to this inquiry? We also have an STS ASE system and were told to never do anything else so as to not disturb the chamber chemistry, but I wonder how critical this really is. Thanks, Jim >Dear colleagues >>From the publication of Ichiki et al. Thin Solid Films 435 (2003) 62-68 >I learned that glas >etching with SF6 and Ar works quiet well. When we bought 4 years ago a >ICP system (STS) >for Si deep etching and a RIE system for glas (resp SiO2, Si3N4) etching >we were told from STS not to do >both processes in the same chamber because of reproducibility. >Does anyone has experience in running glas etch (SF6/Ar) and silicon >deep etching >on the same ICP system. Do I contaminate the si deep etching chamber by >glass etching >or is it possible to clean up the system without open it (no mechanical >clean)? > >Thanks for response. >Greetings >Stefan -- - Jim Beall 303-497-5989 beall@boulder.nist.gov