The Ultrasil Corporation in Hayward California routinely reduces the size of wafers from a larger diameter to a smaller diameter and then re-edge grinds as required. We can do standard material or SOI material. Please contact us for additional information. Tom Gentemann Ph # 510-266-3700 Fax # 510-266-3720 e-mail - ultrasiltg@aol.com