Hi everyone.
I'm having problem coating my glass slide with SU-8 resist. It seems that
the SU-8 does not adhere very well to glass. After developing, some part of
my patterns are lifted off. Does anyone know how to solve this problem? Does
the softbake or PEB have anything to do with this? Thanks.

Abang Annuar