Hi Xiaodong, Wow, very small features! One trick that has worked for us in the past is to run the etch and deposition gases simultaneously. Also, you may have problems with a notch appearing immediately below the oxide. This seems to occur due to local substrate charging. I believe you may have to switch to a resist and control its profile near the etch window to mitigate this effect. -Mike Martin University of Louisville