Hi! I want to use MF319 to develop AZ1518 layer ( I don't want to buy developer if I can...I have AZ 1518 pre-coated wafers). According to the manual I can use most type of positive PR developer.. So, I think I can use MF 319 for my wafer and some paper state that they used MF319 for some AZ1500 series. But the tehnical support person hestitate to say "yes" and instead of say yes they said I can try to develope and then if OK then I can use...... Please answer my question if you know anything about this.... Thanks, sokwon p.s. Has anybody tried to develope SU-8 with acetone?