Hello, has anybody experience in exposing SU-8 using a g-line stepper (the only we can use)? We would need to use thin films (<5µm) of SU-8 for making optical waveguides, but we found no evidence in publications whether the absorption would be enough for a good exposure. Thanks for your comments. Regards Matteo -- Matteo Dainese KTH - Royal Institute of Technology Sweden