Hello, Can anyone sugguest how to get vertical sidewall for 20um thick TOK PMER P-LA900PM photoresist with broadband light source? The strcutre feature size is 10um. I expose this positive resist with a 1:1 projection exposure system. The numerical aperture of the project lens is 0.14 with 30um DOF and 4um resolution. Thanks Ren