Hello guys. I am having difficult time to bond glass to glass. Bottom substrate has 2um wide and deep microfluidic channels and electrodes (Ti/Au 200/1000A). Top substrate is just plain pyrex 7740. I have been trying two methods so far. First one is anodic bonding. I deposited SiO2 on top substrate using Ebeam evaporator. Tried to bond using anodic bond. It did not work. Second method is PDMS to glass bonding. First of all, I spined coat PDMS liquid on top substrate around 6um thickness and curing for 30 min at 180C on hotplate. Cool down it for while. Oxygen plasma treatment on both side of substrate and then place them together. It did not work either. If I miss some steps, please correct me. I will really appreciate if you guys give me any comments or recommendation. Thanks.