With no success I mean poor etching rate. Do you have a good recipe to suggest a solution that can give me a rapid deep (> than 10 micrometers) etching pit? > What do you mean by no success - poor quality or something else? The > type of glass is also relevant. I have had good results with 2% conc. HF > + 2% conc. HNO3 when using soda-lime glass. I have never tried it on > quartz though, but I would not expect it to etch at a similar rate.