Dear all,

I would like to remove positive photoresist after treating sample in RIE.
And I found that it's very difficult to remove the photoresist in acetone.
Then I want to use PRS 2000. But I don't know whether it will attack
the Carbon nanotube in my sample. Does anyone have the experience
or any suggestion about removing PR in the sample with CNT?

Thanks a lot!
Lin Yu