durusmail: mems-talk: PDMS Sealing over Au?!
PDMS Sealing over Au?!
2007-06-21
2007-06-22
2007-06-22
2007-06-22
2007-06-25
PDMS Sealing over Au?!
shay kaplan
2007-06-22
Can you evaporate ti or cr over the gold in the crossing area?

-----Original Message-----
From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org]
On Behalf Of N H
Sent: Thursday, June 21, 2007 8:33 PM
To: mems-talk@memsnet.org
Subject: [mems-talk] PDMS Sealing over Au?!

Hi Dear

I´m having some troubles on sealing PDMS over Au by O2 plasma
activation. As
a mater of fact, I have a PDMS/Glass u-TAS prototype with Au electrode
crossing  the micro-channel array, but when I fill my channels the liquid
leaks trough the Au/PDMS interface and I loss the control over my
electrochemical detection area! Is there someone who could help me to
activate Au surface for making Au/PDMS sealing strong enough?!
reply