A good general resource to check evaporation/sputtering conditions is: http://www.lesker.com/newweb/menu_techinfo.cfm?CFID=1555271&CFTOKEN=59855514&sec tion=materialdeposition&init=skip (if that link isn't permanent, google "lesker material deposition table") Indium has lots of info available. - Kevin ********************************* Kevin Paul Nichols MESA+ Institute for Nanotechnology Mesoscale Chemical Systems Meander 151 University of Twente Postbus 217 7500 AE Enschede The Netherlands Office: +31 (0)53 489 26 31 Mobile: +31 (0)6 49 312 471 Fax : +31 (0)53 489 35 95 Email : k.p.nichols@utwente.nl -----Original Message----- From: mems-talk-bounces@memsnet.org on behalf of jpt sharma Sent: Tue 10/23/2007 8:06 PM To: mems-talk@memsnet.org Subject: [mems-talk] Indium Deposition Hi All I am thinking of depositing indium for metal lift off. I am wondering anyone has done this before? Can we deposit Indium by thermal?