They should be able to give you drills upwards of 1 mil (25.4 microns).

We're currently trying out their drills to drill  7740 glass wafers,
typically to 500 microns


Shekhar


At 10:25 PM 8/13/98 -0400, you wrote:
>Hi folks.
>
>I looking to drill an array of 10umPyrex substrates.
>
>Any takers?
>
>Thanks.
>
>Robert S. Okojie