I am not exactly sure what the poster meant by 'concave'. Here is a
photo. If the structure looks like this, then the problem is
under-exposure. In fact, even the exposed sidewalls are not vertical
because the dose is decreasing with depth.
http://131.238.119.245/sarangan/SU8-profile.jpg