Hi Alim Polat, When foil is really thin you can try to cut it with a lasermarking tool. While using a glasplate to support the foil you are able to transport an remove the foil without damaging it. Regards, Bernd -----Ursprüngliche Nachricht----- Von: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] Im Auftrag von alim polat Gesendet: Dienstag, 16. September 2008 12:18 An: mems-talk@memsnet.org Betreff: [mems-talk] How to cut thin ZnO foil without damaging surfaceroughness and without deformation! Hello Everyone I have this thin ZnO thin film foil and I want to cut it to get mm scale, for example 7 mm x 7 mm without damaging its surface smoothness. So the two important factors are: 1. Surface should stay smooth. No damage to the surface. 2. Also I don't want to deform the surface when I cut it. I really appreciate if you give me some suggestions. Thank you very much. Let's support MEMS-TALK.