Shipley 1165 will remove any of the 18xx series resist even better than acetone, which will generally do the trick (unless you're doing lifoff). Note that 1165 does not mix well with acetone, so its best to rinse it off with water. On Thu, Jun 11, 2009 at 1:18 PM, li xuanwrote: > Hi, > > I am using the shipley 1805 to coat my plate to make hologram. My process is > > 1. coat the glass with 1805, then let it air dry for about 4 days. > 2. make some hologram on it. > 3. silver spray > 4. put into electroforming tank grow to a thick shim. > 5. seperate the shim from the glass. used NaOH 5% to remove the photoresistor from the silver layer. > > Now the problem I got is when I put the silver shim back into tank to make a copy. the copy is always got stick and lots of water strip. People think it is because the photoresistor is not compeletly removed from the silver layer or maybe the silver layer gets destroyed by NaOH. Does anyone have any idea why this happens? Do I really have to bake the photoresistor to make it easy to remove? Can anyone recommend some remover? I try the shipley 1112A. seems does not work at all. Thanks! > > > Paddy