Dear all,

I'm using ebeam evaporation to deposit Ti and Al. Both films have dense
particles observed under microscope. The evporation rates are controlled to
be 4A/s. The wafers were thoroughly cleaned.

What are the reasons that forms the particles? How to solve this problem?

Thank you very much for your suggestions.

cfshen