Peter,

A Google search for Hitachi dry film DFXP10050C1 came up empty.  Is this
film designed for wafer bonding?

Roger Shile

-----Original Message-----
Subject: Re: [mems-talk] thermally curable glue

Hello,

I'm sorry. It wasn't Fuji, but Hitachi dry film.
We used DFXP10050C1.

Regards,

Peter Kuijpers