Hi Prassana,

Thanks a lot for this suggestion. I'm afraid that long-time stability of
this adhesive can't be guaranteed so this unfortunately can't be our final
solution.

But you gave me the idea to use the adhesive you proposed to "pre-adjust"
the two glasses in our bonder at the edges of the glasses. Curing the glue
(dispensed before the pre-adjustment) will happen after that by using an
UV-flood exposure (produced by some UV-tubes).

Subsequently the adhesive will be removed with water... I will check this
out...

Chris