Spray thin carbon nanotube layer? On Wed, Jan 6, 2010 at 8:41 AM, Brad Cantoswrote: > Hi Everyone, and Happy New Year. > > Is anyone aware of a service that can apply a transparent conductive coating to a plastic sheet? This would have to be fairly low temperature process due to the low melting point of the plastic. The sheet resistance requirements are not too rigorous, anything under 400 ohms/square should be fine. Optimally, it would need to be >99% transmissive over 400-1100nm wavelength range, but at this point >80% is acceptable. > > Thanks for your help. > > Brad Cantos > brad.cantos@holage.com > http://holage.com