Hi Jiho,

Xenon Difluoride does not etch plexiglass.

Kyle

 >>  Hello all,

 >>  Do you guys know Xenon Difluoride etches the plexiglass?

 >>  I am planning to bond the molded Si chip with polymer onto the
 >>  plexiglass and put it into the chamber.

 >>  Please let me know if you any ideas.

 >>  Thank you.