Jennifer Lewis at UIUC does something similar, check out her recent publications on direct ink writing with silver: http://colloids.matse.illinois.edu/research.html -Alex On Wed, Sep 29, 2010 at 3:04 PM, Mingke Xiongwrote: > Hi all, > > I am wondering if anyone has some experience with how to make silver nano > paste out of silver nano powder, or maybe has a reference where I can find > such information. > > Our plan is to screen print the silver paste onto PCBs serving as seeding > layer for electroplating. Right now we have some silver nano powders with > 40~90nm dimension. We want to find out what is the best way to disperse the > powder into solvent, a good coating method, proper baking temperature, etc. > > Thank you all in advance. > > Regards, > > Mingke Xiong > AEM, Inc. > 6610 Cobra Way > San Diego, CA 92121, USA > 858-481-0210 (1660) > www.aem-usa.com