Thank you for the information. That really helps. Regards, Mingke Xiong AEM, Inc. 6610 Cobra Way San Diego, CA 92121, USA 858-481-0210 (1660) www.aem-usa.com ________________________________________ From: mems-talk-bounces+mxiong=aem-usa.com@memsnet.org [mems-talk-bounces+mxiong =aem-usa.com@memsnet.org] On Behalf Of Alex Mellnik [arm282@cornell.edu] Sent: Thursday, September 30, 2010 2:20 PM To: General MEMS discussion Subject: Re: [mems-talk] silver nano paste Jennifer Lewis at UIUC does something similar, check out her recent publications on direct ink writing with silver: http://colloids.matse.illinois.edu/research.html -Alex