Hi? This is JIN from UT at Austin. chrome + gold layer can be a mask layer for HF for a long period of time. Good Luck. At 06:08 AM 10/20/98 PDT, you wrote: >Hello Mems Workers > >Could anybody give me any leads on a substance that could be used as a >masking material for HF for a long period of time. > >Thanks in advance > >Julian Shapley >University of Cardiff. >UK > >______________________________________________________ >Get Your Private, Free Email at http://www.hotmail.com > > ************************************************ Seung-Jin Yoo The University of Texas at Austin Microelectronics Reseach Center e-mail:yoosj@ccwf.cc.utexas.edu voice: (office) 512-471-8104 ************************************************