Hi, Peter,

Doesn't silver have the highest electricity conductivity?

Regards,

Mingke Xiong
AEM, Inc.
6670 Cobra Way
San Diego, CA 92121, USA
858-481-0210 ext. 1660
www.aem-usa.com

________________________________________
From: mems-talk-bounces+mxiong=aem-usa.com@memsnet.org [mems-talk-bounces+mxiong
=aem-usa.com@memsnet.org] On Behalf Of Kuijpers, Peter
[p.e.m.kuijpers@philips.com]
Sent: Wednesday, October 27, 2010 12:35 AM
To: General MEMS discussion
Subject: Re: [mems-talk] copper plating

Hi,

Maybe sputtering a thin layer of Cu?

Best regards,

Peter Kuijpers