Hi Xinjie, Google TOPAS or CYTOP for the details of the materials. I think one of them could work. BR, Fei 2011/3/23 Xinjie Song> Dear All, > > I need some help on photoresist/polymer. > > I'm now looking for a type of photoresist/polymer, whose refractive index > is > <1.538 @1.55um cuz i need it to be a cladding layer of a waveguide. The > smaller the refractive index is, the better. Any suggestions, please? > > Thanks in advance > > Xinjie Song, PhD student -- Best regards, Yours sincerely Fei Wang ______________ Assistant Professor, Dr MIC - Department of Micro and Nanotechnology Technical University of Denmark (DTU) Building 344, 1st floor, Room no. 130 DK-2800, Kgs. Lyngby Denmark Tel: +45 4525 6311 Fax: +45 4588 7762 Email: fei.wang@nanotech.dtu.dk http://www.nanotech.dtu.dk