HMDS has worked for me on both Pyrex and Quartz. I suspect it should work on glass just as well. Kipp On Tue, Mar 6, 2012 at 4:37 PM, Xiaohui Linwrote: > hi all: > > Could any one suggest how to improve the adhesion of SU8 2005 to glass > or quartz? > > I tried glass+omnicoat+SU8, it is week. I also tried > quartz+omnicoat+SU8 , but still peel off when I put in plating solution > (pH=5). > > Will HMDS work? or other adhesion promoter? > > thanks > _______________________________________________ > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > provider of MEMS and Nanotechnology design and fabrication services. > Visit us at http://www.mems-exchange.org > > Want to advertise to this community? See http://www.memsnet.org > > To unsubscribe: > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > -- _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk