35:20 ratio of (85% phosphoric acid):(chromic acid) @ 80C from J. Electrochem. Soc., Volume 106, Issue 6, pp. 481-485 (1959) It wasn't a MEMS application, but they used Al foil, and then anodized, and selectively (and slowly) etched away the oxide they formed on top of it for TEM analysis of the oxide film. On Wed, Jun 20, 2012 at 5:44 AM, Ned Flanderswrote: > Does it exist? > If it etches alumina and not aluminum at all, it gets extra magic points. > > > Help? > _______________________________________________ > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > provider of MEMS and Nanotechnology design and fabrication services. > Visit us at http://www.mems-exchange.org > > Want to advertise to this community? See http://www.memsnet.org > > To unsubscribe: > http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk