Hi, Have you tried sulphuric acid at elevated temperature say 70-80C ? Best Regards, Ricky Anthony Ph.D. Student Microsystems Center Tyndall National Institute University College Cork Cork, Ireland ________________________________________ From: mems-talk-bounces+ricky.anthony=tyndall.ie@memsnet.org [mems-talk- bounces+ricky.anthony=tyndall.ie@memsnet.org] on behalf of Gianmario Scotti [gianmario.scotti@gmail.com] Sent: 04 November 2013 17:18:32 To: General MEMS discussion Subject: Re: [mems-talk] Etching of ALD titania (TiO2) I only need to etch 50 nm, but HF doesn't work with ALD TiO2 - it doesn't etch it at all. On Sat, Nov 2, 2013 at 12:30 AM, 조명래wrote: > I Am not sure how much the thickness you wanna etch. How about starting > with conventional titanium etchant? Of course HF based etchant is dangerous > but it surely have selectivity over Si. > 2013. 11. 1. 오전 8:22에 "Gianmario Scotti" 님이 > 작성: > > > Dear MEMS researchers, > > > > > > do you know of a wet etchant that would remove ALD TiO2 from silicon? > Some > > of my colleagues told me that they don't know of anything suitable for > ALD > > films of TiO2 - only TiO2 nanoparticles. Incredulous, I hit google, but > > came up with nothing - apparently, continuous films of TiO2 are quite a > > challenge to etch with wet etchants. > > > > Would any of you have a recipe that was tested as working with ALD TiO2? > > > > > > > > Cheers! > > > > -- > > Gianmario Scotti > > > > Researcher > > Aalto University, Dept. of Materials Science and Engineering > > http://materials.aalto.fi/en/ > > > > Micronova, Tietotie 3 > > 02150 Espoo > > Finland > > _______________________________________________ > > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > > provider of MEMS and Nanotechnology design and fabrication services. > > Visit us at http://www.mems-exchange.org > > > > Want to advertise to this community? See http://www.memsnet.org > > > > To unsubscribe: > > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > > > _______________________________________________ > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > provider of MEMS and Nanotechnology design and fabrication services. > Visit us at http://www.mems-exchange.org > > Want to advertise to this community? See http://www.memsnet.org > > To unsubscribe: > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > -- Gianmario Scotti Researcher Aalto University, Dept. of Materials Science and Engineering http://materials.aalto.fi/en/ Micronova, Tietotie 3 02150 Espoo Finland _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk