===== Original Message from mems-talk@memsnet.org at 12/26/01 6:10 pm >HI, Does anyone have a detailed protocol for bonding glass to glass? We >have been trying to bond while maintaining an optical quality surface >(pure thermal bonding doesn't seem to work) and we haven't had luck with >applying a voltage across the glass with temp around 400 degrees. We're >using pyrex right now (borofloat, specifically). Any suggestion would be >appreciated. > >Thanks, > >Ziggy >_______________________________________________ >mems-talk@memsnet.org mailing list: to unsubscribe or change your list >options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk >Hosted by the MEMS Exchange, providers of MEMS processing services. >Visit us at http://www.mems-exchange.org/ ===== Comments by jintrater@integer-eng.com ("Jim Intrater -- IE") at 12/27/01 1:32 pm There are such things as optical adhesives, but they probably won't withstand 400 degrees.