durusmail: mems-talk: Anodic bonding glass-titanium
Anodic bonding glass-titanium
2002-03-01
2002-03-01
2002-03-01
2002-03-05
Anodic bonding glass-titanium
Islam Rafiqul
2002-03-01
Can you provide the details of your process?
Temperature?
Voltage
time?
etc...

Best Regards,
Rafiqul Islam


EV Group Inc.- Technology- Tel: (602) 437 9492 x 118, (602)2842134
(cell),Fax: (602) 437 9435,
e-mail: R.Islam@EVGroup.com web: www.EVGroup.com


-----Original Message-----
From: lteyssed@altern.org [mailto:lteyssed@altern.org]
Sent: Friday, March 01, 2002 3:06 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] Anodic bonding glass-titanium


I tried to make anodic bonding between glass and titanium but it was
unsuccessful.  Have you any idea about why it didn't succeed ?

Thank you in advance.
_______________________________________________
mems-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply