Abhinav Bhushan
2002-03-01
can you divulge some details of the process?
temperature, thickness of Ti layer, cleaning method,
time, force, contact area, glass type...

Abhinav

--- lteyssed@altern.org wrote:
> I tried to make anodic bonding between glass and
> titanium but it was unsuccessful.  Have you any idea
> about why it didn't succeed ?
>
> Thank you in advance.