hi all, We are looking for etching a 4000 A polysilicon layer. We want the etching do be completed in less then 2min as there after our photoresist tend to etch away. So what solution shd we try and what proportion. Thanks Regards Abhay Porwal __________________________________________________ Do you Yahoo!? Yahoo! Mail Plus - Powerful. Affordable. Sign up now. http://mailplus.yahoo.com