durusmail: mems-talk: thickness restriction of photosensitive Polyimide
thickness restriction of photosensitive Polyimide
2003-02-24
the relationship between backing temperature and time and post treatments such as exposure or developing
2003-02-25
2003-02-24
thickness restriction of photosensitive Polyimide
Houri Johari
2003-02-24
Dear all,
Is there any limitation for the thickness of photosensitive polyimide
(ultradel 7501)?
Is there any available source for the limitation in the thickness of
different photosensitive polyimide, at all?
Thanks
Houri
reply