I found the cracking issue of SU-8 during development process.
I also found the some delamination together on Au sputtered wafer.
If you have any experience of this issue, please share your experience and your
solution.
Any information will be appreciated.

Thanks.

YOON,  IME(Institute of Microelectronics), Singapore