Hi Mohamed, BCB will not withstand the etch. Shay Mohamed Saadoui wrote: > Hi, > > I want to use CYCLOTENE resine BCB-4000 as protective coating during silicon > etching in pottasium hydroxide KOH at 85C, which must be removed at the end of > processing. > > It will be very helpful if anyone can give information about this BCB process. > > Thanks and Regards, > > Mohamed SAADAOUI > Laboratoire d' Analyse > et d' Architectures Systemes > LAAS- TOULOUSE. france > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/